搜索
Highpuritylithiummetal&Lithiumalloy
Lithium foil
Thickness (0.02mm-50mm) x width (4mm-400mm).


Lithium alloy ingots
We can develop binary, ternary or quaternary alloys according to the phase diagram.


Lithium Boron Alloy chip
Lithium-boron alloy chips
Physical Characteristics
Molecular formula: Li , B
Phase composition:Li7B6▪nLi
Melting point: ≥600℃
Part No.#:Li55,Li60,Li65,Li70
Chemical Index
Part No.#
Chemical Composition(weight) /%
Li
Other
Li 55
55±2
remainder
Li 60
60±2
remainder
Li 65
65±2
remainder
Li 70
70±2
remainder
Specifications
The dimensions and tolerances are as follows, and the specific specifications are customized according to customer's requirements. (Unit: mm)
Diameter
Diameter Tolerance
Thickness
Thickness Tolerance
4.0-16
±0.1
0.1-0.3
±0.01
>16-21
±0.2
>0.3-0.6
±0.02
>21-100
±0.3
>0.6-0.8
±0.02
>0.8-1.0
±0.03
>1.0-2.0
±0.04
Performance Introduction
1. Compared with the widely used lithium-silicon alloy, lithium-boron alloy has better performance in terms of maximum voltage and discharge time as an anode material.
2. Under different loads, the maximum voltage of the unit battery is 0.10-0.27V higher than that of lithium-silicon alloy, and the discharge time is extended by 11.4-78.1%.
Appearance Quality
The surface of the product shall be:
-Clean and bright
-Free of dark spots or surface depressions that would cause scrap
-Free of oxidation
-Free of foreign matter
Edges shall be smooth and free from burrs
Inner & Outer Packaging
Inner packaging: Metal cans or aluminum plastic composite bags, filled with high-purity argon gas for packaging.
Outer packaging: Corrugated cardboard boxes or steel drums.
Transportation/Storage Conditions
1. During the transportation of the product, it should be fireproof and moisture-proof, and should not collide violently. Drums should not roll on the ground.
2. The product should be stored in a rain-proof, clean, dry, non-corrosive and well-ventilated environment. It is strictly prohibited to store in the open storage.
3. The shelf life of the product is 1 year.


lithium-magnesium alloy foil
Mg content 1.0-30.0wt% , Li remainder.


Lithium-aluminum alloy foil
Al content 0.1-5.0wt% , Li remainder.


Lithium granule
diameter (2mm-20mm) x length (1mm-50mm)


Previous page
1
2
3
Next page
China Energy Lithium Foil Co., Ltd
Company Tel:+86 22 59832337,59832338,59832339
Sales Tel:+86 22 59816838,59816832,59816829
E-mail:cel@cellithium.com
Company address: No. 100, the 9th Avenue of Xinye, West TEDA, Tianjin, China.